SAE J 404-2009 SAE合金钢的化学成分
百检网 2021-07-15
标准号:SAE J 404-2009
中文标准名称:SAE合金钢的化学成分
英文标准名称:Chemical Compositions of SAE Alloy Steels
标准类型:H40
发布日期:2009/1/27 12:00:00
实施日期:1999/12/31 12:00:00
中国标准分类号:H40
国际标准分类号:77.080.20
引用标准:ASTM A 506-2005;ASTM A 507-2006;ASTM A 513-2008;ASTM A 519-2006;SAE J 408-1983;SAE J 409-1995;SAE J 1081-2000;SAE J 1249-2008;SAE J 1268-1995;SAE J 1868-1993
适用范围:In 1941, the SAE Iron and Steel Division in collaboration with the American Iron and Steel Institute (AISI) made a major change in the method of expressing composition ranges for the SAE steels. The plan, as now applied, is based in general on narrower ladle analysis ranges plus certain product (check) analysis allowances on individual samples, in place of the fixed ranges and limits without tolerances formerly provided for carbon and other elements in SAE steels (reference SAE J408). ISTC Division 1 has developed a procedure which allows for the maintenance of the grade list in this SAE Standard. This will involve conducting an industry-wide survey to solicit input. This survey will be conducted at a frequency deemed necessary by the technical committee. Criteria have been established for the addition to or deletion of grades from the grade table. A new grade will be considered if it meets standard SAE grade ranges, has a minimum usage or production of 225 tonnes/year (250 tons/year), and has the endorsement of at least two users or producers. New steel compositions will still be considered as Potential Standard (PS) steels, based on the guidelines provided in SAE J1081, until such time as production of the new steel achieves a level of production or usage qualifying it for consideration as a standard steel. The deletion of a grade from the grade table will be by consensus based on the grade survey results. Deleted grades will be archived in SAE J1249 for future reference. The compositions in this document may apply to open hearth and basic oxygen, or electric furnace steels. Grades shown in Table 1 with prefix letter E are normally made by the electric furnace process with maximum limits of 0.025% phosphorus and 0.025% sulfur. The nominal chemical limits or ranges in the compositions given in Table 1 are subject to standard variations in check analysis given in SAE J409. Since AISI is no longer issuing steel grade designations, all grades listed in this document are SAE grades.
百检能给您带来哪些改变?
1、检测行业全覆盖,满足不同的检测;
2、实验室全覆盖,就近分配本地化检测;
3、工程师一对一服务,让检测更精准;
4、免费初检,初检不收取检测费用;
5、自助下单 快递免费上门取样;
6、周期短,费用低,服务周到;
7、拥有CMA、CNAS、CAL等权威资质;
8、检测报告权威有效、中国通用;