SAE AMS 5662M-2004 自耗电极或真空感应熔炼1775°F (968℃)固溶热处理沉淀硬化的含52.5Ni-19Cr-3.0Mo-5.1Cb (Nb)-0.90Ti-0.50Al-18F
百检网 2021-08-02
标准号:SAE AMS 5662M-2004
中文标准名称:自耗电*或真空感应熔炼1775°F (968℃)固溶热处理沉淀硬化的含52.5Ni-19Cr-3.0Mo-5.1Cb (Nb)-0.90Ti-0.50Al-18Fe耐腐蚀和耐热的镍合金棒材,锻件和环件
英文标准名称:Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 52.5Ni 19Cr 3.0Mo 5.1Cb (Nb) 0.90Ti 0.50Al 18Fe, Consumable Electrode or Vacuum Induction Melted 1775°F (968°C) Solution Heat Treated, Precipitation Hardenable
标准类型:V11
发布日期:2004/7/12 12:00:00
实施日期:1999/12/31 12:00:00
中国标准分类号:V11
国际标准分类号:49.025.15
引用标准:ASTM E 8-2004;ASTM E 8M-2004;ASTM E 10-2001;ASTM E 21-2003;ASTM E 103-1984;ASTM E 112-1996;ASTM E 139-2000;ASTM E 292-2001;ASTM E 354-1993;SAE AMS 2261;SAE AMS 2261G-2002;SAE AMS 2269E-1994;SAE AMS 2371G-2003;SAE AMS 2374D-2002;SAE AMS 2750C-1990;SAE AMS
适用范围:This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging flash welded rings or heading. These products have been used typically for parts requiring high resistance to creep and stress-rupture up to 1300 degrees F (704 degrees C) and oxidation resistance up to 1800 degrees F (982 degrees C), particularly those parts which are formed or welded and then precipitation heat treated to develop required properties, but usage is not limited to such applications.
百检能给您带来哪些改变?
1、检测行业全覆盖,满足不同的检测;
2、实验室全覆盖,就近分配本地化检测;
3、工程师一对一服务,让检测更精准;
4、免费初检,初检不收取检测费用;
5、自助下单 快递免费上门取样;
6、周期短,费用低,服务周到;
7、拥有CMA、CNAS、CAL等权威资质;
8、检测报告权威有效、中国通用;
相关商品
C,S,Mn,Si,P,Cr,Ni,W,Mo,V,Al,Ti,Cu,Nb,Co,B,Zr,As,Sn JIS G0320:2017 《钢材的炼钢化学成分分析方法》 JIS G0320:2017
Si,Mn,P,Cr,Ni,Co,Cu,Mo,V,Ti,Al KS D1673-2007 《钢铁 感应结合等离子发光分光分析方法》 KS D1673:2007